2.4694 Nickel Alloy Technical Specifications

Standards

Mat. No. 2.4694
EU NiCr16Fe7TiAl
AISI/ASTM -
UNS N07751
Other Inconel Alloy 751
Alloy 751
Nicrofer 7016 TiAl
The 2.4694 / Alloy 751 alloy is similar to the Alloy X-750 alloy. Only the aluminum content has been increased for better precipitation hardening.
600 °It maintains high tensile strength up to C temperature. °It exhibits high creep and fatigue resistance up to 820C temperature. °It has high oxidation resistance up to 980C temperature. It has high resistance to stress corrosion at low and high temperatures. It has good weldability.

Chemical Composition & Mechanical and Physical Properties

C% 0.10 max
Mn% 1.00 max
Ti% 2.00-2.60
S% 0.010 max
Si% 0.50 max
Cr% 14.00-17.00
Ni% 70.00 min
Nb% 0.70-1.20
Cu% 0.50 max
AI% 0.90-1.50
Fe% 5.00-9.00
0.2% Yield Strength Rp N/mm2 716 min
Tensile Strength Rm N/mm2 1172 min 1080 min
Elongation A5 % 24 min
Tensile Strength (1000 hours)
650 °C 280 MPa
730 °C 240 MPa
815 °C 97 MPa
Solution Annealed ve precipitation hardened.

Application areas

In combustion chambers and exhaust valves.