Alloy 825 Nickel Alloy Technical Specifications

Standards

Mat. No. 2.4858
EU NiCr21Mo
AISI/ASTM -
UNS N08825
Diğer Inconel 825
Nicrofer 4221
Alloy 825
2.4858 / Alloy 825 is a nickel-chromium-iron alloy containing stabilized copper and molybdenum.
It is highly resistant to reducing and oxidizing acids, stress corrosion cracking, as well as localized corrosion such as pitting and crevice corrosion. It is particularly resistant to phosphoric acid and sulfuric acid.

Chemical Composition & Mechanical and Physical Properties

C% 0.025 max
Mn% 1.00 max
P% 0.020 max
S% 0.015 max
Si% 0.50 max
Cr% 19.50-23.50
Ni% 38.00-46.00
Mo% 2.50-3.50
Cu% 1.50-3.00
AI% 0.20 max
Co% 1.00 max
Ti% 0.60-1.20
Fe% Rest
0.2 % Yield Strength Rp N/mm2 240 min
Tensile Strength Rm N/mm2 550 min
Elongation A5 % 30 min
Elastic Modulus kN/mm2 195

Application areas

In chemical processes, nuclear fuel reprocessing, oil and gas piping.

Specifications

BS 3072 – BS 3074, 3076 (NA16)
ASTM B 163, B 366, B 423 – B 425, B 564, B 704, B 705, B 751, B 775, B 829
NACE MR-0175/ISO 15156
ASME SB-163, SB-366, SB-423 – SB-425, SB-564, SB-704, SB-705, SB-751, SB-775, SB-829
DIN 17744, 17750 – 17754 ISO 6207, 6208, 9723 – 9725